產品列表PRODUCTS LIST
本頁面標準信息均來源于網絡收集,或由參與標準制定的供應商提供,只作為參考使用,為確保測試結果的準確性、節省您的時間,如需VDA 621-415標準詳細信息或VDA 621-415具體測試方法,請與我們技術人員聯系或給我們留言,我們將為您提供相關的技術支持。
This test procedure has been developed to judge the corrosion protection of vehicle paint using an accelerated laboratory test. It is claimed that testing according to this procedure can generate results that correlate well with those seen by driven vehicles. This test is cyclic in nature, i.e.; test specimens are exposed to changing climates over time.
Test specimens are placed in an enclosed chamber and exposed to a changing climate that comprises of the following 3 part repeating cycle. 24.0 hours exposure to salt spray according to DIN 50 021-SS. This is followed by 96.0 hours exposure to a condensing water climate according to DIN 50 017-KFW. This is followed by 48.0 hours exposure to an ambient climate of +18 to +28C according to DIN 50 014. The number of cycle repeats and therefore the test duration is variable.
Please see elsewhere in this document for details of DIN 50 021-SS, DIN 50 017-KFW & DIN 50 014.
This test is also referred to as a Cyclic Corrosion Test, often abbreviated to CCT.